7. Workshop Conditions
Keep the workshop clean and free from dust. Remove grinding dust as it occurs. The working area
must not be affected by draughts.
The workshop temperature must be maintained:
%
)
for L285 between 18 °C (65 °F) and 27 °C (80 °F).
%
)
for RIM 935 between 18 °C (65 °F) and 23 °C (73 °F).
%
The temperature must not fall below 15 °C (59 °F).
%
The relative humidity during mixing, applying or curing resins must not be allowed to rise above 80%
%
for L285 or 65% for RIM 935.
%
Maintain the workshop temperature as near to 25 °C (77 °F) as possible during curing.
Summary of Contents for DA 42 NG
Page 933: ...AIRCRAFT DA 42 NG AMM Fuel Doc 7 02 15 Rev 4 28 TITLE Page 1 15 Mar 2018 CHAPTER 28 FUEL ...
Page 1459: ...AIRCRAFT DA 42 NG AMM Lights Doc 7 02 15 Rev 4 33 TITLE Page 1 15 Mar 2018 CHAPTER 33 LIGHTS ...
Page 1711: ...AIRCRAFT DA 42 NG AMM Doors Doc 7 02 15 Rev 4 52 TITLE Page 1 15 Mar 2018 CHAPTER 52 DOORS ...
Page 1853: ...AIRCRAFT DA 42 NG AMM Wings Doc 7 02 15 Rev 4 57 TITLE Page 1 15 Mar 2018 CHAPTER 57 WINGS ...
Page 2071: ...AIRCRAFT DA 42 NG AMM Engine Doc 7 02 15 Rev 4 72 TITLE Page 1 15 Mar 2018 CHAPTER 72 ENGINE ...
Page 2288: ......
Page 2320: ......
Page 2322: ......