NetCol5000-A020 Air Cooled In-row Precision Air
Conditioner
User Manual
3 Installation Guide
Issue 01 (2014-06-30)
Huawei Proprietary and Confidential
Copyright © Huawei Technologies Co., Ltd.
42
Figure 3-23
Welding refrigerant pipes
(1) Discharge pipe
(2) Suction pipe
During the welding process, charge a little nitrogen into the pipes to avoid impurity caused by
internal oxidation, as shown in
Figure 3-24
.
Slowly charge nitrogen into pipes through the high-pressure needle valve when welding
gas pipes.
Slowly charge nitrogen into pipes through the liquid needle valve when welding liquid
pipes.
Figure 3-24
Welding schematic diagram
Step 2
Take out two straight pipes in the fitting bag, which are of an outer diameter of 5/8 inch and
1/2 inch respectively. Weld the straight pipes at the positions, as shown in
Figure 3-23