26
MD 610_2d 11/2019
Aluminium
with Vario Powder Pack
0.01 – 0.25 mg/l Al
Use two clean vials (24 mm Ø) and mark one as blank
for zeroing.
1.
Fill
20 ml of the water sample
in a 100 ml beaker.
2. Add the contents of
one Vario Aluminum ECR F20
Powder Pack
straight from the foil to the water sample.
3.
Dissolvethe powder using a clean stirring rod.
4.
Press
[ ]
key.
Wait for a
reaction period of 30 seconds.
After the reaction period is finished proceed as follows:
5.
Add the contentsof
one Vario Hexamine F20 Powder
Pack
straight from the foil to the same water sample.
6.
Dissolvethe powder using a clean stirring rod.
7. Add
1 drop of Vario Aluminum ECR Masking
Reagent
in the vial marked asblank.
8.
Add 10 ml of the preparedwater sampleto the vial (this
is the blank).
9.
Add the remaining 10 ml of the preparedwater sample
in the second clean vial (this is the sample).
10. Close the vials tightly with the caps and swirl several
times to mix the contents.
11. Press
[ ]
key.
Wait for
a reaction period of 5 minutes
.
After the reaction period is finished proceed as follows:
12. Place the vial (the blank) in the sample chamber
making sure that the
marks are aligned.
Countdown 1
0:30
start:
Countdown 2
5:00
start:
1
2
3
4
5
0
Summary of Contents for Lovibond MD 610
Page 14: ...8 MD 610_2d 11 2019...
Page 15: ...9 MD 610_2d 11 2019 Part 1 Methods...
Page 87: ...81 MD 610_2d 11 2019...
Page 95: ...89 MD 610_2d 11 2019...
Page 306: ...300 MD 610_2d 11 2019...
Page 307: ...301 MD 610_2d 11 2019 Part 2 Instrument Manual...
Page 310: ...304 MD 610_2d 11 2019...
Page 362: ...356 MD 610_2d 11 2019...