(2)
It refers to the cracks occuring on weld seams or spot weldings:
(a) clean thê surface along the crack in order to remove previous weld seam;
(b) weld the crack, do not clean the weld seam;
NOTE: It is admissible to correct the weld seams twice.
(3) Type of welding: electrical shielded arc welding with use of argon, welding wire Ø1 mm of material 1H18N10T, current
intensity 35A.