12.11.2 Removal and Installation
12.11.2.1 Plastic Repair Notices
1. Apply protective cream to any exposed skin to avoid skin
irritation.
2. Wear rubber gloves.
3. When use compressed air or sanding, wear protective
goggles.
4. Remove any mixture that comes into contact with skin
immediately, as the mixture will become solid very quickly.
5. When grinding or sanding, wear a dust mask and protective
goggles.
6. Wash the skin with cold water to minimize irritation caused
by resin dust.
7. Avoid dropping repair materials onto clothes.
8. Use repair materials in a well ventilated environment, as the
dust produced during repairs is toxic.
9. After use, close all the repair material containers. Dust or
moisture will contaminate the repair materials and weaken
the repair quality.
12.11.2.2 Thermosetting Plastic Dent Repair
1. Clean the area to be repaired.
2. Heat the dent part with a blower until the appropriate tools
can be used to press flat the dent.
3. Grind the dent area with sandpaper/emery paper.
4. Clean the dent area with cleaning agent and leave it dry 5
min.
5. Apply a thin layer of adhesive and leave it dry 10 min.
6. Fill the uneven surface with adhesive and smooth out with
putty knife.
7. Use an infrared light to accelerate the curing process and
raise the temperature to 60-70°C (140-158 ºF), heat 15 min.
8. Polish the dent area with sanding paper.
9. Remove dust debris.
10. Apply a thin layer of adhesive and leave it dry 10 min.
11. Restore the plastic surface according to the plastic surface
repair process.
12.11.2.3 Thermosetting Plastic Scratch
Repair
1. Clean the area to be repaired.
12-110
Plastic Panel Information and Repair
Body, Sheet Metal and Painting
EC718/EC718RV EC715/EC715RV 10/2009
Summary of Contents for EC715 2009
Page 4: ......
Page 330: ...Next Step 10 End 2 248 Fuel System JL4G18 D Engine EC718 EC718RV EC715 EC715RV 10 2009 ...
Page 1164: ......
Page 2008: ......