8.1.4.2.6 Weld seam end
All welding procedure parameters that affect the downslope phase at the weld seam end can be set in
the "Downslope" section of the welding procedure. The settings can prevent the formation of an end
crater.
43
44
45
Illustration: "Downslope" section of the welding procedure
NO.
PARAMETER
FUNCTION
43
"Downslope Time" Time period in seconds of linear current reduction, starting from the welding
current value of the previous level, until the set final current is reached.
44
"Final Current"
Value of the final current in amperes, when it is reached during current re-
duction, the welding arc is extinguished.
45
"Rotate During
Downslope"
The "Rotate During Downslope" function can be used to set the rotation be-
havior of the weld head rotor during the final slope.
"Rotate During Downslope"
"ON"
Electrode is moved at the welding speed of
the previous level during the final slope.
"Rotate During Downslope"
"OFF"
Electrode remains in place during the final
slope.
Summary of Contents for MOBILE WELDER OC PLUS
Page 8: ...ENGLISH MOBILE WELDER OC PLUS 8 ORBITALUM TOOLS GmbH D 78224 Singen www orbitalum com ...
Page 20: ...ENGLISH MOBILE WELDER OC PLUS 20 ORBITALUM TOOLS GmbH D 78224 Singen www orbitalum com ...
Page 177: ...MOBILE WELDER OC PLUS ENGLISH ORBITALUM TOOLS GmbH D 78224 Singen www orbitalum com 177 ...
Page 200: ...SPARE PARTS MOBILE WELDER OC PLUS 200 ORBITALUM TOOLS GmbH D 78224 Singen www orbitalum com ...
Page 204: ......