Hot wires can be used to cure a delamination with minor affect on the
cosmetics of the part.
•
Five-minute epoxy, superglue or molten ICW06 can be used to repair
broken models.
•
In addition to D-Limonene, chemicals such as Tetrahydrofuran (THF),
Methyl Chloride, and Trichloroethylene are solvents for ICW06, but all
should be used with extreme caution.
Moving the Z Stage While Modeling
Stratasys recommends that you do not move the Z stage while building
models. Moving the Z stage causes the model to be inaccurate because
the FDM modeler does not keep its last Z stage position in its memory.
Summary of Contents for FDM 2000
Page 1: ...Introduction FDM 2000 3000 8000 Release 2 0 Stratasys Document no 105208 0001 Rev B...
Page 17: ...Contents FDM 2000 3000 8000 Manual 10 MAY 01 F2 3 8000 vi...
Page 105: ...Reference N 2 Notes 10MAY01 Release 1 0 October 1997 5 0 May 2001...
Page 131: ...G 1 Reference Glossary 10MAY01 Release 4 0 Glossary Stratasys Document no 105213 0001 Rev B...