9. WELDING PREPARATION
(Continued)
9.4 Welding Conditions
When setting to the improper welding conditions, the following troubles will occur.
Cause
Trouble
Wire extension is too long.
・
Long Arc length
・
Wide bead width
・
Poor shield
・
current increase Note 1
Wire extension is too short.
・
Short arc length
・
Easy generation of spatter
・
current decrease
Note 1
Welding voltage is too high.
・
Long arc length
・
Wide bead width
・
Shallow penetration and flat bead
Welding voltage is too low.
・
Stick to base metal and easy generation of spatter
・
Narrow bead width
・
Deep penetration and high excess metal
Welding current is too high.
・
Wide bead width
・
Deep penetration and high excess metal
Welding speed is too fast.
・
Narrow bead width
・
Shallow penetration and low excess metal
The data in the tables below is only for reference. Please find the optimum welding conditions for
weldment shape and welding position.