G.10
TE 250R - 310R 2013 I.E. / TE 310R 2013 I.E. USA
TC 250R 2013 - TC 250R 2013 I.E. USA
TXC 250R - 310R 2013 I.E. USA
ENGINE OVERHAUL
Workshop Manual Ed. 07-2012
Cylinder
Check the walls for dents or scuffing. Measure cylinder bore diameter at three
different positions. Measure each diameter in two directions at right angles to
each other to determine taper and out-of-round.
Max. taper: 0.05 mm.
Max. out-of-round: 0.05 mm.
If cylinder is worn beyond these limits, replace both cylinder and piston. The liner
undergoes a special hardening treatment and cannot be ground.
Piston
Clean off any carbon deposits from piston crown and grooves. Perform a careful
visual inspection of the piston and check its dimensions. There should be no
signs of forcing, scuffing, cracking or other damage.