22
optics11.com
3.
USING THE PIUMA NANOINDENTER
This section describes the use of the Piuma Nanoindenter after having prepared the instrument for
a measurement (Chapter 2).
3.1
Stage controls
The motorized stages of the Piuma can be manually positioned in X, Y and Z directions, each having
a travel of 12000 mm. To use the stages to position the area of interest under the Piuma probe tip,
start by bringing the probe in the field of view. To do so, move the manual stage all the way up to
avoid damaging the probe, and use the Z-stage to bring down the probe into the field of view of
the on-
board camera. Put a travel value in the ‘Travel’ field, such as 500 µm, and press the ‘down’
arrow of the Z-stage to move this amount down (Figure 17).
Figure 17: Main software window: Stage controls (red), Piezo controls/Position information (green). The probe is brought
into the camera image, close to the focal plane, using the down arrow of the Z-stage.
Optical
calibration
Geometrical
factor
Measurement
Summary of Contents for CHIARO NANOINDENTER
Page 1: ...PIUMA NANOINDENTER USER MANUAL ...
Page 63: ...63 Flowchart Calibration ...
Page 65: ......