Inspecting the Heater Filaments
3. Verify the outer filament is not in contact with the liner for the heater assembly.
4. Check all the standoffs and ceramics for damage.
5. Record the general condition of the chamber and flow flange, looking for any damage or other
abnormal conditions.
Deposition should be even around the chamber wall, and primarily it occurs below the plane of the
wafer carrier.
Uneven deposition on the reactor wall usually indicates an imbalance in the gas flow.