OM-2226 Page 70
14-9. Groove (Butt) Joints
S-0062
1
Tack Welds
Prevent edges of joint from draw-
ing together ahead of electrode by
tack welding the materials in posi-
tion before final weld.
2
Square Groove Weld
Good for materials up to 3/16 in. (5
mm) thick.
3
Single V-Groove Weld
Good for materials 3/16
−
3/4 in.
(5-19 mm) thick. Cut bevel with
oxyacetylene or plasma cutting
equipment. Remove scale from
material after cutting. A grinder
can also be used to prepare bev-
els.
Create 30 degree angle of bevel
on materials in V-groove welding.
4
Double V-Groove Weld
Good for materials thicker than
3/16 in. (5 mm).
30
°
2
1
1/16 in.
(1.6 mm)
3
4
14-10. Lap Joint
S-0063 / S-0064
1
Electrode
2
Single-Layer Fillet Weld
Move electrode in circular motion.
3
Multi-Layer Fillet Weld
Weld a second layer when a heavi-
er fillet is needed. Remove slag
before making another weld pass.
Weld both sides of joint for maxi-
mum strength.
30
°
Or Less
30
°
Or Less
1
1
2
3
14-11. Tee Joint
S-0060 / S-0058-A / S-0061
1
Electrode
2
Fillet Weld
Keep arc short and move at defi-
nite rate of speed. Hold electrode
as shown to provide fusion into the
corner. Square edge of the weld
surface.
For maximum strength weld both
sides of upright section.
3
Multi-Layer Deposits
Weld a second layer when a heavi-
er fillet is needed. Use any of the
weaving patterns shown in
Section 14-8. Remove slag before
making another weld pass.
45
°
Or
Less
1
2
1
3
2
Summary of Contents for Maxstar 200 DX
Page 6: ...Notes...
Page 16: ...OM 2226 Page 10...
Page 65: ...OM 2226 Page 59 SECTION 8 ELECTRICAL DIAGRAMS Figure 8 1 Circuit Diagram 237 566 B...
Page 79: ...OM 2226 Page 73 Notes...
Page 89: ...OM 2226 Page 83 Notes...