61
8.
FAQ & TROUBLESHOOT
Q1: The automated find-surface function fails to detect the surface automatically.
A1: The Piuma looks for a voltage difference when using the find-surface function. In case any
problems occur with the find-surface function, please verify the signal amplitude on the OP1550 is
sufficient (absolute values 3-7 V minimum, or an amplitude of 4V or higher). Please check whether
the piezo BNC cable is properly connected. If the problem persists, verify the probe is not too stiff
for the sample, and check the probe for contamination under a (stereo) microscope.
Q2: I only get ‘noise’ data after performing an indentation.
A2: Check if the ‘Modulation’ box in the ADC menu of the OP1550 is ticked. In case the problem
persists, check the probe for contamination under a (stereo) microscope.
Q3: I get more cantilever bending than displacement in the results (a backward sloping load-
displacement curve).
A3: Verify the probe is calibrated in the medium the probe is used in. In case this is uncertain,
recalibrate the probe on a stiff surface. Also, please ensure the tip hits the sample prior to any other
part of the cantilever hitting the sample. In case the problem persists, check the probe for
contamination under a (stereo) microscope.
Q4: The Piuma stage motors keep on moving
during the initial ‘homing’ procedure
when starting
up the software.
A4: If the X, Y-stages fail to reach starting positions during the homing procedure, this indicates
something obstructs the stage. Take off the protector stage or backlight module and check whether
the X-Y stage is free to move.