18
optics11.com
Figure 11: Automatic optical signal calibration, displayed in the Piuma software.
This process must be performed for each new medium/probe combination: to measure multiple
samples in a solution of which the refractive index is not significantly different, this procedure does
not have to be executed again.
When performing experiments with temperature control, the calibration should be accomplished at
the same temperature as the measurement temperature. This is because the refractive index of the
medium is dependent on the temperature. Since the density of a liquid usually decreases with
temperature, it is not surprising that the speed of light in a liquid will normally increase as the
temperature increases. Thus, the index of refraction normally decreases as the temperature
increases for a liquid.