52
MAIN process
5.7.2 Normal CW
This is a MIG/MAG welding process without pulse but with synergy func-
tion. The welding current depends on the distance between torch and
workpiece. In connection with the QIROX robot application, arc seam track-
ing is possible to a limited extent. This welding process is suitable for sheet
thicknesses from 0.5 mm - 3.0 mm.
5.8 Rapid Weld
The Rapid Weld process generates a very concentrated arc during the weld-
ing process, which guarantees a very deep penetration.
The following characteristic curves are available as Rapid Weld variant:
• Normal, Fe, 92 % Ar, 8 % CO
2
, wire 1.0 mm
• Normal, Fe, 92 % Ar, 8 % CO
2
, wire 1.4 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 0.8 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.0 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.2 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.4 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.6 mm
• Normal, Fe, 91 % Ar, 4 % O
2
, 5% CO
2
, wire 1.2 mm
• Normal, Fe, 91 % Ar, 4 % O
2
, 5% CO
2
, wire 1.4 mm
• Normal, Fe, 91 % Ar, 4 % O
2
, 5% CO
2
, wire 1.6 mm
To activate the Rapid Weld characteristic curve, you have to select one of
the above mentioned characteristic curves and the variant 1 M or Rapid
Weld at the PREMIUM operating module.
(Main/Synergy/Variant --> variant 1 M).
INFO!
Summary of Contents for QINEO
Page 4: ......
Page 10: ......
Page 11: ...11 Operational safety Block 1 Operational Safety...
Page 29: ...29 Block 2 Basic information Qineo Champ Pro...
Page 42: ...CHAMP Pro 42...
Page 109: ...109 Block 4 Additional information...
Page 124: ...124 SD module...
Page 138: ...138 Commissioning 6 7 8 5...
Page 140: ...140 Commissioning 7 5 6 The wire inlet must not touch the wire drive roller INFO...
Page 145: ...145 Block 6a Error messages...
Page 159: ...159 Block 6b General maintenance instructions...
Page 164: ...164...
Page 165: ...165 Block 7 Automation...
Page 184: ...184...
Page 185: ...185...
Page 186: ...www qineo de...