HEATING MAIN MONTAGE INSTRUCTIONS CV4.04
Fill sleeve with PUR foam components
only after cooling of the sleeve down to
the surrounding temperature.
11. In separate containers pour components “A" and "B" in quantities that are specified in
Addition Nr 5 tables.
Pour component "A" and then component "B" in one container and for not longer than
15 minutes mix rapidly the component.
Within 30 seconds pour mixed component in the drilled hole, Ø 25 mm in diameter.
If components "A" and "B" are in separate containers and are for only one connection,
then pour component "B" into the container with component "A", mix rapidly and pour
into the drilled hole with diameter of Ø 25 mm.
12. Close drilled hole with PE cork.
13. After PUR foam hardening (not earlier
than in 2,5 hours) cut cork top part,
clean PE sleeve surface from dust and
foam remains around drilled holes ( ~70
mm in radius). Heat up to 60°C using
weak flame area around cork for the
FOPS patch.
14. Heat sticky side of the patch for about 1-
3 sec. and press it against the cork.
Heat the patch with weak flame until
green indicator on the patch is gone.
It is not allowable for glued patch to
have any air entrapped underneath it or
have corners bent up. Around the patch
side wide region of glue should be
seen.
8.1.5.