Fig. 6.7.1-1: Battery
• Measure the electrolyte density of individual cells with a
commercial hydrometer. The hydrometer reading (see table
on following page) indicates the battery’s state of charge.
During measurement, the temperature of the electrolyte
should preferably be 20
°
C.
Attention
The gases emitted by the battery are explosive! Keep sparks
and naked flames away from the battery!
Do not allow battery acid to come into contact with skin or clot-
hing!
Wear protective goggles!
Do not rest tools on the battery!
6.8
Grease lubricated generator backend bearing
A bearing change should only be executed by a trained expert.
The bearing is, depending on the generator model, equipped with a black cooling disc.
The grease lubricated generator bearing is maintenance free over its durability, but should be exchanged every
1500 operating hours.
Fig. 6.8-1: Fettgeschmiertes Backendlager
Grease lubricated backend bearing without cooling disc.
Sample Picture
Electrolyte density
in [kg/ l]
Charge status
Normal
Tropical
1.28
1.23
well charged
1.20
1.12
semi-charged, re-charge
1.12
1.08
discharged, immediately charge
Содержание 10000 NE
Страница 26: ...Seite Page 26 General R01 1 11 3 11 Leere Seite Intentionally blank General References and Regulations...
Страница 162: ...Seite Page 162 Panda PMS 8 000 NE 42 NE Manual R05 11 3 11 Leere Seite Intentionally blank Generator Faults...
Страница 208: ...Seite Page 208 Panel Generator Control P6 RE0703_Kunde_eng R06 1 11 3 11 Leere Seite Intentionally blank Measurements...