Print More Materials, All For Application
- 27 -
4.4 Disassembly Model
Step 1
the finished model on the
printing platform
Step 2
Turn off the vacuum adsorption
switch
Step 3
After taking down the platform,
carefully shovel the model from all
sides slowly
4.5 PEEK Material Printing Precautions
Materials/Parameters Printing Temp Platform Temp
Chamber Temp
Z-axis support spacing
peek
400
100
90-120
0.15-0.2
Note:
1. Peek can only be printed with high temperature head. Brim is recommended for attachment mode
2. When heating before printing, the constant temperature chamber and hot bed should be heated first. The
printing head should not be heated for a long time. It is easy to form carbonization and lead to the blockage of
the printing head (
see common problems and solutions for the blockage treatment - PEEK printing
).
3. PEEK should be baked at 120℃ for 5H before printing
4. The cooling fan is turned off when printing
Содержание HIGH-TEMPERATURE Series
Страница 7: ...Print More Materials All For Application 7 2 Detailed Parameter 2 1 Specification ...
Страница 8: ...Print More Materials All For Application 8 ...
Страница 10: ...Print More Materials All For Application 10 Internal Chamber ...
Страница 11: ...Print More Materials All For Application 11 Filament Box Electric Box Pressure Gauge Air Pump Cooling Fan ...
Страница 12: ...Print More Materials All For Application 12 Cooling Fan Built In Light Built In Camera Motor Power Outlet ...