Design and function
MIG/MAG welding
099-005444-EW501
17.03.2015
63
5.10.9.3 Example, tack welding (non-latched)
Figure 5-32
Basic parameters
Parameter
Meaning / explanation
Setting range
GASstr
Gas pre-flow time
0.0s to 20.0s
GASend:
Gas post-flow time
0.0s to 20s
RUECK
Wire burn-back length
2 to 500
"P
A
" main program
Parameter
Meaning / explanation
Setting range
Setting the wire speed
5.10.9.4 Example, aluminium tack welding (non-latched special)
Figure 5-33
Basic parameters
Welding parameter Meaning / explanation
Setting range
GASstr
Gas pre-flow time
0.0s to 20.0s
GASend:
Gas post-flow time
0.0s to 20.0s
RUECK
Wire burn-back length
2 to 500
"P
START
" start program
Welding parameter Meaning / explanation
Setting range
DVstart
Wire speed
0% to 200%
Ustart
Arc length correction
-9.9V to +9.9V
tstart
Duration
0.0s to 20s
"P
A
" main program
Welding parameter Meaning / explanation
Setting range
Setting the wire speed
"P
END
" end-crater program
Welding parameter Meaning / explanation
Setting range
DVend
Wire speed
0% to 200%
Uend
Arc length correction
-9.9V to +9.9V
tend
Duration
0.0s to 20s