Arc characteristics adjustment
This section explains the adjustment procedure of arc characteristics (arc status). Using this function enables to adjust the
arc status into soft or hard condition.
1.
HOME > Arc characteristic
2.
Set the arc characteristic.
3.
Select OK.
The arc characteristic set values are registered and the screen returns to the previous one.
T I P S
•
It is likely that good weld can be obtained by adjusting it to "hard" in low current region and
"soft" in high current region.
•
When using an extended cable for the base material side /torch side or using an extended
torch cable, it is likely that good welding can be performed by adjusting it to "hard."
Summary of Contents for OTC ARXIS pulse P403L
Page 1: ...July 2023 Manual No P30433 1 DAIHEN Corporation ARXIS pulse P403L P503L OWNER S MANUAL...
Page 174: ...REFERENCE DRAWING REFERENCE MATERIALS CHAPTER 10 172 10 2 1 Schematic diagram ARXIS WB P403L...
Page 175: ...REFERENCE DRAWING REFERENCE MATERIALS CHAPTER 10 173 Chapter 10 Reference Materials...
Page 176: ...REFERENCE DRAWING REFERENCE MATERIALS CHAPTER 10 174 ARXIS WB P503L...
Page 177: ...REFERENCE DRAWING REFERENCE MATERIALS CHAPTER 10 175 Chapter 10 Reference Materials...