OM-253 918 Page 44
B. Stick (SMAW) Welding
Trouble
Remedy
Hard starts, poor welding characterist-
ics, unusual spattering.
Use proper type and size of electrode.
Check electrode polarity and reverse in necessary; check and correct poor connections
Make sure a remote control is not connected.
C. TIG (GTAW) Welding
Trouble
Remedy
Wandering arc, hard starts, poor welding
characteristics, spattering problems.
Use proper type and size of tungsten.
Use properly prepared tungsten.
Check electrode polarity and reverse if necessary.
Tungsten electrode oxidizing and not
remaining bright after welding.
Shield weld zone from drafts.
Check for correct type shielding gas.
Check and tighten gas fittings.
Check electrode polarity and reverse if necessary.
Содержание MPi 220P
Страница 6: ......
Страница 51: ...OM 2253 918 Page 45 Notes...
Страница 52: ...OM 253 918 Page 46 SECTION 7 ELECTRICAL DIAGRAMS Figure 7 1 Circuit Diagram For Welding Power Source...
Страница 53: ...OM 2253 918 Page 47 956142882 B...