42
Cause
Pieces to be welded too big.
Solution
Increase the welding current.
Slag inclusions
Cause Poor
cleanliness.
Solution
Clean the pieces accurately before welding.
Cause
Electrode diameter too big.
Solution
Use a smaller diameter electrode.
Cause
Incorrect edge preparation.
Solution
Increase the chamfering.
Cause
Incorrect welding mode.
Solution
Decrease the distance between the electrode and
the piece.
Move regularly during all the welding operations.
Blowholes
Cause
Insufficient shielding gas.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Sticking
Cause
Incorrect arc length.
Solution Increase the distance between the electrode and
the piece.
Increase the welding voltage.
Cause
Incorrect welding parameters.
Solution
Increase the welding current.
Cause
Incorrect welding mode.
Solution
Angle the torch more.
Cause
Pieces to be welded too big.
Solution
Increase the welding current.
Increase the welding voltage.
Cause
Incorrect arc regulation.
Solution
Increase the equivalent circuit inductive value setting.
Undercuts
Cause
Incorrect welding parameters.
Solution
Decrease the welding voltage.
Use a smaller diameter electrode.
Cause
Incorrect arc length.
Solution Increase the distance between the electrode and
the piece.
Increase the welding voltage.
Cause
Incorrect welding mode.
Solution
Decrease the side oscillation speed while filling.
Decrease the travel speed while welding.
Cause
Insufficient shielding gas.
Solution
Use gases suitable for the materials to be welded.
Oxidations
Cause
Insufficient gas protection.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Porosity
Cause
Grease, varnish, rust or dirt on the workpieces to
be welded.
Solution
Clean the workpieces carefully before welding.
Cause
Grease, varnish, rust or dirt on the filler material.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Humidity in the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Incorrect arc length.
Solution
Decrease the distance between the electrode and
the piece.
Decrease the welding voltage.
Cause
Humidity in the welding gas.
Solution
Always use quality materials and products.
Ensure the gas supply system is always in perfect
condition.
Cause
Insufficient shielding gas.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Cause
The weld pool solidifies too quickly.
Solution
Decrease the travel speed while welding.
Pre-heat the workpieces to be welded.
Increase the welding.
Hot cracks
Cause
Incorrect welding parameters.
Solution
Decrease the welding voltage.
Use a smaller diameter electrode.
Cause
Grease, varnish, rust or dirt on the workpieces to
be welded.
Solution
Clean the workpieces carefully before welding.
Cause
Grease, varnish, rust or dirt on the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Incorrect welding mode.
Solution
Carry out the correct sequence of operations for
the type of joint to be welded.
Cause
Pieces to be welded have different characteristics.
Solution
Carry out buttering before welding.
Cold cracks
Cause
Humidity in the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Particular geometry of the joint to be welded.
Solution
Pre-heat the pieces to be welded.
Carry out post-heating.
Carry out the correct sequence of operations for
the type of joint to be welded.
For any doubts and/or problems do not hesitate to contact
your nearest customer service centre.
Summary of Contents for WF 230 Classic
Page 70: ...70...
Page 202: ...202...
Page 224: ...224...
Page 246: ...246...
Page 250: ...250 1 3 1 4 11 35 1 5...
Page 251: ...251 1 6 1 7 EN IEC 60974 10 B A A EN60974 10 A pace maker...
Page 253: ...253 3 kit a e oyap MIG MAG 4 5 5 6 7 5 15 3 3 1 WF 230 MIG MAG Quasar 3 2 WF 230 Classic...
Page 263: ...263 4 8 Kit RC WF Exclusive 73 11 015 kit a e oyap 4 9 Roll bar kit a e oyap 5 6...
Page 264: ...264 Reset encoder...
Page 265: ...265...
Page 266: ...266 7 7 1 MMA Hot Start Arc Force antisticking...
Page 267: ...267 7 2 MIG MAG MIG SHORT ARC 1a SHORT a SPRAY ARC b SPRAY ARC 1b 2 3 2 3 1a 1b...
Page 270: ...270...
Page 274: ...274 WF 230 Exclusive...
Page 278: ...278 07 01 601 SL 2R 2T...
Page 281: ...281...
Page 282: ...282 2X M6 2X M6x30mm...
Page 283: ...283 73 11 015 WF Exclusive Kit RC 2X M3 9x9mm...
Page 284: ...284 71 03 036 Roll bar 4X M6 4X M6x20mm 1X D10mm d7mm 1X M5x60mm...