Over Extrusion
If there is excess filament coming out of the hot end, follow the steps below.
1.
Reduce the extrusion percentage on the Printer Control Screen or Web Interface.
Note: Filament diameters can occasionally be over diameter.
First Layer Not Sticking to Bed
If the first layer is not sticking to the print bed, confirm the following items:
✓
The bed temperature is at the correct temperature.
o
If not, wait until the temperature is met.
Note: The bed can be preheated to the print temperature to allow for extra time for
heat to transfer from the heater to the build plate.
✓
An approved material is being used.
✓
The end of the nozzle is clean of excess material.
✓
The nozzle is properly gapped to 0.2 mm.
✓
The bed is level.
o
This can be done by quickly checking the four corners with the Check Bed
Level macro or run Quick Level macro.
✓
The filament is dry.
o
Consult the manufacturer for the appropriate drying procedure.
✓
The bed is residue free.
o
The bed can be cleaned with isopropyl alcohol
TIP: Lightly rough the bed surface with 200 grit sandpaper if necessary.
Print Sagging or Drooping
If the print is sagging or drooping, review the geometry of the model. With a 2 mm nozzle,
the maximum printable overhang angle with PCTG is 55°.
Summary of Contents for Emergence PRO
Page 1: ...Emergence PRO 3D Printer Operation Manual Revision C INNOVATION PRECISION EXCELLENCE ...
Page 62: ...Emergence PRO 3D Printer Manual Revision C December 2020 Page 62 of 68 Figure 58 Print Head 1 ...
Page 63: ...Emergence PRO 3D Printer Manual Revision C December 2020 Page 63 of 68 Figure 59 Print Head 2 ...