OPERATION
HPR130 Manual Gas
Instruction Manual
4-23
0
Damage
Replace swirl ring
Dirt or debris
Clean and check for damage, and replace swirl ring
if damaged
Gas holes
Blocked holes
Replace swirl ring
O-rings
1. Damage
Replace swirl ring
2. Lubricant
Apply a thin film of silicone lubricant if dry
Inspect consumables
Part
Check for
Action
Cap
Nozzle
Swirl ring
Electrode
Center surface
Wear
O-rings
1. Damage
Replace electrode*
2. Lubricant
Apply a thin film of silicone lubricant if dry
*Always replace the nozzle and electrode as a set.
Center hole
1. Must be round
Replace nozzle if hole is no longer round*
2. Signs of arcing
Replace nozzle*
O-rings
1. Damage
Replace nozzle*
2. Lubricant
Apply a thin film of silicone lubricant if dry
Erosion or missing material
Replace nozzle*
Blocked gas holes
Replace nozzle*
Erosion, missing material
Replace cap
Cracks
Replace cap
Burned
Replace cap
See
Inspect electrode pit depth
later in
this section
Summary of Contents for HPR130
Page 1: ...Manual gas Instruction manual 804570 Revision 6 HyPerformance Plasma HPR130 ...
Page 40: ...SPECIFICATIONS 2 2 HPR130 Manual Gas Instruction Manual 5 ...
Page 132: ...MAINTENANCE HPR130 Manual Gas Instruction Manual 5 9 PCB block diagram 3 ...
Page 146: ...MAINTENANCE HPR130 Manual Gas Instruction Manual 5 23 CNC operation with pump timeout 5 ...
Page 151: ...MAINTENANCE 5 28 HPR130 Manual Gas Instruction Manual 6 Coolant flow troubleshooting chart ...
Page 195: ...HPR130 Manual Gas Instruction Manual 7 5 Discrete output functionality ...
Page 238: ......
Page 239: ......