Electrode preparation for DC welding
The electrode should be pointedaccording to the welding current.
Angle @
[°]
Range of current
[ A ]
30
60-90
90-120
120
0-30
30-120
120-250
>250
TYPES OF ELECTRODES
ELECTRODE
COLOUR
USE
Cerium-Tungsten
Grey
Universal
Thorium Tungsten
Red
Fe-Stailess steel-Copper
Welding Position
Place the tip at 3-4 mm (.12 - .16in) from the weld piece, press the torch trigger, the arc will automatically ignite; as
soon as the bath forms, move slowly and with constant speed so as to produce a bath that is uniform in penetration
and width.
If filling material is used, keep the rod at a slope and about 20 mm (.79in) from the piece; when the weld pool
becomes fluid, move the torch back and add material, touching the rod to the pool. (Filling material is always
necessary for aluminium.)
Pull the rod away and position the torch back near the weld bead.
Repeat this operation quickly and constantly so that the weld remains homogenous.
Содержание Ergus WIG 160 CDI
Страница 1: ...MANU 115 M TIG 00 INDUSTRIE LINE WIG 160 DCi CDI WIG 201 DCi CDI USER MANUAL...
Страница 23: ...23 BLOCK DIAGRAM WIG 160 DCi...
Страница 24: ...24 WIG 160 CDI...
Страница 25: ...25 WIG 201 DCi...
Страница 26: ...26 WIG 201 CDI...
Страница 27: ...27 REMOTE CONTROL CONNECTION DIAGRAM WIRING OF CONNECTORS...
Страница 29: ...29 WIG 160 DCi...
Страница 31: ...31 WIG 160 CDI...
Страница 33: ...33 WIG 201 DCi...
Страница 35: ...35 WIG 201 CDI...