3.7 Welding techniques
TIG Welding techniques
60–75°
15–30°
Nozzle
Direction of travel
Welding Rod
Shield gas
Vertical
Tungsten electrode
The suggested electrode and welding rod angles for welding a bead on
plate are shown above. The same angles are used when making a butt
weld. The torch is held 60–75° from the metal surface. This is the same
as holding the torch 15–30° from the vertical.
Take special note that the rod is in the shielding gas during the
welding process.
3.8 Torch movement during welding
Tungsten Without Filler Rod
Tungsten With Filler Rod
75°
75°
15°
Welding
direction
Form pool
75°
75°
15°
Welding
direction
Form pool
75°
75°
15°
Tilt torch
75°
75°
15°
Tilt torch
75°
75°
15°
Move torch to front of pool. Repeat.
75°
75°
15°
Add filler metal
75°
75°
15°
Remove rod
75°
75°
15°
Move torch to front of pool. Repeat.
21
BOC Smootharc 180 Multiprocess operating manual
Содержание 180 Multiprocess
Страница 1: ...180 Multiprocess Operating manual 6PRRWKDUF GYDQF GYDQF ...
Страница 45: ...45 BOC Smootharc 180 Multiprocess operating manual ...
Страница 53: ......
Страница 54: ......
Страница 55: ......