49
OM-405
12.13 Weld Test
S-0057-B
1
Vise
2
Weld Joint
3
Hammer
Strike weld joint in direction shown.
A good weld bends over but does
not break.
2 To 3 in
1/4 in
3
2
1
2 To 3 in
3
2
1
(51-76 mm)
(6.4 mm)
(51-76 mm)
12.14 Troubleshooting – Porosity
Porosity – small cavities or holes resulting from gas
pockets in weld metal.
Possible Causes
Corrective Actions
Arc length too long.
Reduce arc length.
Damp electrode.
Use dry electrode.
Workpiece dirty.
Remove all grease, oil, moisture, rust, paint, coatings, slag, and dirt from work surface before
welding.
12.15 Troubleshooting – Excessive Spatter
Excessive Spatter – scattering of molten metal particles
that cool to solid form near weld bead.
Possible Causes
Corrective Actions
Amperage too high for electrode.
Decrease amperage or select larger electrode.
Arc length too long or voltage too high.
Reduce arc length or voltage.
Содержание Bobcat 225 NT
Страница 4: ......
Страница 39: ...35 OM 405 10 Electrical Diagrams 10 1 Circuit Diagram For Welding Generator Onan Powered Units SB 180 688...
Страница 40: ...36 OM 405 10 2 Circuit Diagram For Welding Generator Kohler Powered Units SB 183 459 A...
Страница 65: ...61 OM 405 Notes...
Страница 70: ...Notes...
Страница 71: ...Notes...
Страница 72: ...Notes...