THERMO-LAG 3000 APPROVED PRIMERS
•
CARBOGUARD 888
•
CARBOGUARD 890
•
CARBOGUARD 893 SG
•
CARBOMASTIC 15
•
CARBOMASTIC 242
•
CARBOZINC 858
•
CARBOZINC 859
•
RUSTBOND
(Interior only and 2.0 mils max.)
•
CARBOZINC / RUSTBOND
(THE PRIMER SYSTEM THICKNESS RANGE SHALL BE BETWEEN 3 – 5 MILS (75 – 125
MICRONS) (DFT) PER SSPC PA 2. ANY OTHER DRY FILM THICKNESS IN EXCESS OF
THIS VALUE SHALL BE AGREED UPON BY CARBOLINE IN WRITING – PRIOR TO START
UP OF THE PROJECT)