113
(30) Tappet
Mainly check the tappet contact surface with the cam and
push rod. Slight surface defects shall be corrected with
an oilstone.
(a) Tappet stem outside diameter measurement
mm
4.4.6 Cylinder bore correction
1) Slight uneven worn, flawed, etc. shall be corrected
by honing only. If the cylinder is unevenly worn
partially, flawed or otherwise damaged and cannot be
repaired simply by honing, rebore the cylinder first and
then hone. See 4.4.5.(1)(c) for the boring dimension.
2) Items to be prepared for honing
Flex-Hone
(see No.8 of 4.1.2 in Chapter 4)
Electric
drill
Honing
fluid
(50:50 mixture of lube oil and diesel oil)
Model
Item
Standard
Limit
Tappet
hole I.D.
12.000 12.025
12.04
5
Stem O.D. 11.975 11.990
11.95
5
3/4IRH8N
Clearance
0.010 0.050
0.090
Tappet
hole I.D.
12.000 12.018
12.03
8
Stem O.D. 11.975 11.990
11.95
5
4IRI8N
Clearance
0.010 0.043
0.083