0-5461 5-13 OPERATION
Description
Possible Cause
Remedy
5 A groove has been formed in the base
metal adjacent to the toe of a weld
and has not been filled by the weld
metal (undercut).
A Welding current is too high.
A Reduce welding current
B Welding arc is too long.
B Reduce the length of the
welding arc
C Angle of the electrode is
incorrect.
C Electrode should not be
inclined less than 45° to the
vertical face
D Joint preparation does not
allow correct electrode angle.
D Allow more room in joint
for manipulation of the
electrode.
E Electrode too large for joint.
E Use smaller gauge
electrode.
F Insufficient deposit time at
edge of weave.
F
Pause for a moment at
edge of weave to allow weld
metal build-up.
Art # A-07714
Figure 5-31: Examples of undercut
Summary of Contents for WELDSKILL 180
Page 20: ...SERVICE MANUAL 180 INTRODUCTION 2 8 0 5461 This Page Intentionally Blank ...
Page 24: ...SERVICE MANUAL 180 INSTALLATION 3 4 0 5461 This Page Intentionally Blank ...
Page 28: ...SERVICE MANUAL 180 OPERATION 4 4 0 5461 This Page Intentionally Blank ...
Page 54: ...SERVICE MANUAL 180 ROUTINE SERVICE REQUIREMENTS 7 4 0 5461 This Page Intentionally Blank ...
Page 56: ...THEORY OF OPERATION 8 2 0 5461 SERVICE MANUAL 180 This Page Intentionally Blank ...
Page 76: ...KEY SPARE PARTS 13 2 Manual 0 5461 SERVICE MANUAL 180 This Page Intentionally Blank ...
Page 79: ...SERVICE MANUAL 180 This Page Intentionally Blank ...