Strike weld joint in direction shown.
A good weld bends over but does
not break.
2 To 3 in
1/4 in
3
2
1
2 To 3 in
3
2
1
(51-76 mm)
(6.4 mm)
(51-76 mm)
12-14. Troubleshooting – Porosity
Porosity – small cavities or holes resulting from gas
pockets in weld metal.
Possible Causes
Corrective Actions
Arc length too long.
Reduce arc length.
Damp electrode.
Use dry electrode.
Workpiece dirty.
Remove all grease, oil, moisture, rust, paint, coatings, slag, and dirt from work surface before
welding.
12-15. Troubleshooting – Excessive Spatter
Excessive Spatter – scattering of molten metal particles
that cool to solid form near weld bead.
Possible Causes
Corrective Actions
Amperage too high for electrode.
Decrease amperage or select larger electrode.
Arc length too long or voltage too high.
Reduce arc length or voltage.
Содержание Bobcat 250 NT
Страница 32: ...OM 4403 Page 28 7 2 Maintenance Label Onan Powered Units...
Страница 45: ...OM 4403 Page 41 Notes...
Страница 46: ...OM 4403 Page 42 SECTION 10 ELECTRICAL DIAGRAMS Figure 11 1 Circuit Diagram For Welding Generator...
Страница 47: ...OM 4403 Page 43 202 547 D...
Страница 78: ......