![Kamatec PlastoFused Скачать руководство пользователя страница 17](http://html1.mh-extra.com/html/kamatec/plastofused/plastofused_instruction-manua_3316477017.webp)
17
HINT: Don`t use to excessive temperatures. But set
the temperatur high enought to get a melting bath
nevertheless.
8.1
REPAIRING HOLES
Grind off the material on both sides so that there is no
other material in the damaged area.
Start fusing the Melting-Stips with the body-part on the
unpainted inner surface.
Use the adherence roller to fill the hole with the warm
Melting-Strip.
HINT: Use more Melting-Strips near to each other at
larger holes. Please observe in this case, to set the
Melting-Strips imbricate for stronger holding.
Now melt the Melting-Strips from outside.
Let the plastic cool down.
HINT: Arrange the Melting-Strips crosswise to get
a stronger holding.
8.1.1
8.1.2
8.1.3
8.1.4
8.1.5
Allow the plastic to cool down.
Grind the Surface slowly.
8.1.6
8.1.7
8.1.8