11 Materials
Temperatures and the heatbed treatment before print according to a specific material.
11.1 ABS
ABS is very strong and versatile material with
great thermal resistance
. It’s suitable for
both indoor and outdoor use.
ABS is a thermoplastic polymer, that means that just like PLA, it can be melted and
crystallized multiple times without degrading too much. ABS, however, melts at a higher
temperature than PLA. Higher melting temperature gives ABS great thermal resistance, your
prints won’t show signs of deformation
up to 98 °C
.
ABS includes high wear resistance synthetic rubber, which makes it
very strong and
impact resistant
. And last but not least, it’s
soluble in acetone
! This makes it really easy to
not only connect multiple parts together but also allows you to
smooth prints
with acetone
vapors. You still have to be careful when handling acetone, but it’s not anywhere near as
dangerous as for example PLA solvents.
The best use of ABS is architectural models, concept models, spare parts (car
interior, gears, phone cases), etc.
On the other hand, thermal contraction is where ABS makes it really hard to successfully
print something. And that’s especially true when printing anything big. Even with the heatbed
at 100 °C, your part may start lifting from the build plate and warp. This and the
unpleasant
smell
of ABS is why you should consider getting an enclosure for your printer when printing
with ABS. Or at least place the printer in a warm room.
If you need to use your print outside or just need your print stronger, give ABS a shot. It’s
what
LEGO
is made of after all.
ADVANTAGES
DISADVANTAGES
High impact and heat resistance
Bad smell
Strong and versatile
Worse resolution
Soluble in acetone (easy post-processing)
Needs warm room or enclosure
Can be vapor smoothed
● Nozzle temperature:
255
°C
● Bed temperature:
100 °C. You can set the bed temperature between 80 to 110 °C
depending the size of an object (larger object means higher temperature)
● Heatbed:
Make sure the surface is clean as described in
6.3.2 PEI print surface
preparation
chapter
50
Содержание Original Prusa i3 MK2S 1.75mm
Страница 1: ......
Страница 25: ...Pict 11 Probe response diagram Now you are done 25 ...
Страница 61: ...Pict 35 Nozzle change 61 ...