6. Malfunctions Analyses and Solutions
6.1
Frequent joints quality problems analyze
:
Visually check
:
round bead, good joint
Narrow and fall bead. Too high pressure while
welding
Too small bead. Pressure is not enough while
welding
◆
There is a ditch between the welding surfaces.
Temperature is not enough or change-over time is too
long while welding.
◆
High & low bead. Different heating time or fusion
temperature causes that.
◆
Misalignment. Welding under the condition that the
misalignment exceeds 10% of pipe wall thickness