4.3 Possible causes for dissatisfying casting results
Dissatisfying casting results can have various causes and, depending on the material,
can have various effects. The following "check list" is to help find the different causes:
1. Casting temperature is too low/too high.
2. Flask temperature is too low/too high.
3. Configuration of flask is disadvantageous ("branches" too thin or too close to
the top).
4. Flask is not totally heated up (at least 2 hours on end temperature).
5. Flask was slaked too early/too late.
6. Contamination in the alloy (for example "bad copper").
7. Material was not pre-alloyed/granulated.
8. Investment for flask was bad/old
9. Eventually not enough protective gas or the gas had water inclusions.
10. Wrong crucible position (different crucible temperatures).
11. Not enough vacuum inside the vacuum chamber (at least - 0.9 bar for good
casting).
12. Vacuum was turned on too late/turned off too early.
13. Contamination in the investment because of wax residues (steam out flasks).
14. Graphite contamination (use ceramic insert or crucible of better graphite quality).
Please note that INDUTHERM cannot be held responsible for dissatisfying casting
results.
Summary of Contents for VC 400 LCD
Page 27: ...86014010_04_OPERATING_MANUAL_VC400_LCD_GB DOC 25 11 2016 KS page 27 4 4 Configuration of flask...
Page 37: ...86014010_04_OPERATING_MANUAL_VC400_LCD_GB DOC 25 11 2016 KS page 37...
Page 38: ...86014010_04_OPERATING_MANUAL_VC400_LCD_GB DOC 25 11 2016 KS page 38 7 Connection diagrams...
Page 39: ...86014010_04_OPERATING_MANUAL_VC400_LCD_GB DOC 25 11 2016 KS page 39...
Page 40: ...86014010_04_OPERATING_MANUAL_VC400_LCD_GB DOC 25 11 2016 KS page 40...