![GYS 061835 Instruction Manual Download Page 35](http://html1.mh-extra.com/html/gys/061835/061835_instruction-manual_2281106035.webp)
35
NEOPULSE 220 C / 220 C XL
EN
Energie
Hold
Thermal coeff.
See chapter «ENERGY MODE» on pages
following.
MIG-MAG WELDING
• GMAW/MIG-MAG Manual
Settings
Designation
Adjustable
settings
Description & advice
Wire speed
0.5 - 20m/min
Quantity of filler metal deposited and indirectly the welding intensity.
Voltage
10 - Umax
Sets the welding power.
Self
-4 > +4
Smoothes more or less the welding current. To be adjusted according to the welding
position.
Pre-gas
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Post gaz
0 - 25 secs.
Duration for which gas is released after the arc has stopped. It protects the weld pool
and the electrode against oxidisation when the metal is cooling down.
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.
• Standard MIG-MAG/GMAW
(Dynamic STD)
The Standard mode allows high quality welding on most ferrous materials such as steel, stainless steel, but also copper and its alloys, titanium... The
many possibilities of current and gas management allow you to perfectly control your welding operation, from the priming to the final cooling of your
weld bead.
Settings
Designation
Adjustable
settings
Description & advice
Thickness
0.1 - 5.5 mm
The synergy allows for fully automatic settings. Adjusting the thickness
automatically sets the right voltage and wire speed.
Speed
0.5 - 20m/min
Quantity of filler metal deposited and indirectly the welding intensity.
Current
15 - Imax
The welding current is adjusted according to the type of wire used and the material to
be welded.
Arc length
-6 > +6
Used to adjust the distance between the end of the wire and the weld (voltage adjust
-
ment).
Self
-4 > +4
Smoothes more or less the welding current. To be adjusted according to the welding
position.
Pre-gas
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Approach speed
50 - 200 %
Progressive wire speed. Before the arcing, the wire arrives slowly to create the first
contact without causing a jolt.
Hot Start
50 - 200 %
The Hot Start is an overcurrent during generated during the arcing phase to prevent
the wire from sticking. It is adjustable in intensity (% of welding current) and time
(seconds).
0 - 5 secs.
Crater Filler
50 - 100 %
This current treshold when stopped is a phase after the current downslope.
It is adjustable in intensity (% of welding current) and time (seconds).
Post gaz
0 - 25 secs.
Duration for which gas is released after the arc has stopped. It protects the weld pool
and the electrode against oxidisation when the metal is cooling down.
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.