SERVICING INFORMATION 7-9
BATTERY
Complaint
Symptom and possible causes
Remedy
“Sulfation”, acidic
white powdery sub-
stance or spots on
surfaces of cell plates
1. Cracked battery case
2. Battery has been left in a run-down condition for a long
time.
Replace the battery.
Replace the battery.
Battery runs down
quickly.
1. Trouble in charging system
2. Cell plates have lost much of their active material as a
result of overcharging.
3. Internal short-circuit in the battery
4. Too low battery voltage
5. Too old battery
Check the generator, regulator/
rectifier and circuit connections
and make necessary adjust-
ments to obtain specified
charging operation.
Replace the battery, and cor-
rect the charging system.
Replace the battery.
Recharge the battery fully.
Replace the battery.
Battery “sulfation”
1. Incorrect charging rate
(When not in use battery should be checked at least
once a month to avoid sulfation.)
2. The battery was left unused in a cold climate for too
long
Replace the battery.
Replace the battery if badly
sulfated.
Содержание RV125
Страница 1: ...9 9 5 0 0 3 1 2 3 3 0 1 E...
Страница 34: ...PERIODIC MAINTENANCE 2 21...
Страница 56: ...3 20 ENGINE CRANKSHAFT Remove the crankshaft with the special tool 09920 13120 Crankcase separator...
Страница 174: ...6 6 ELECTRICAL SYSTEM CHARGING SYSTEM Generator Regulator rectifier SCR IG switch Battery Load SCR SCR SCR SCR Fuse IC...
Страница 191: ...ELECTRICAL SYSTEM 6 23 SPEEDOMETER Disassemble the speedometer as follows...
Страница 241: ...8 10 RV125K4 K5 04 05 MODELS REAR FENDER INSTALLATION 6 5 N m 0 65 kgf m...
Страница 250: ...Prepared by 2nd Ed January 2006 1st Ed January 2003 Part No 99500 31233 01E Printed in Japan 256...
Страница 251: ...Printed in Japan K3 K4 K5 K6...