• Silicates and Oxides—Silica scale is virtually impossible to remove. Silica
scale is unlikely if SiO
2
is held below 150 ppm. Oxides, such as iron oxide,
can coat all parts of the system if soluble iron is present in concentrations
above 0.5 ppm. Iron oxides do not usually develop into thick scales but can
accentuate the development of other scales.