5.5 PEEK Material Printing Precautions
Material/Parameter
Print Temperature
Platform Temperature
Chamber Temperature
peek
440
100
90
Attention:
1. PEEK can only use high-temperature head printing
2.Pre-heat before printing, should first heat the thermostat chamber and hot bed, the
print head should not be heated for a long-time, long-time heating is easy to form
carbonization lead to print head clogging
(clogging treatment see common problems
and their solutions - PEEK printing)
3. Before printing the material should first use 120 ℃ baking 5H
4. printing when the cooling fan off