Figure 37: First Layer is Too Close
This image shows a first layer that is too close. The infill traces are bonded to their neighbors, but we can see
excess plastic that accumulates above the infill traces. This is less of a problem than a first layer that’s too tall. But
in extreme cases, the print head and bed can be so close than no plastic is extruded at all. This can cause problems
with the extruder slipping or jamming.
To correct this, the corner bolts should be tightened (threaded in clockwise).
Figure 38: First Layer is Correct
This last image shows a “perfect” first layer. The infill traces are firmly bonded to each other, but we see no excess
plastic building up between them.
This graphic from MatterHackers may also be helpful in understanding what the first layer does:
Содержание F306 Generation I
Страница 7: ...7 4 General Info Hardware 4 1 Machine Overview Figure 5 Front View Figure 6 Side View...
Страница 8: ...8 Figure 7 Axes Layout Figure 8 Control Board Detail...
Страница 9: ...9 Figure 9 Print Head Detail Figure 10 Extruder Cold End Detail...
Страница 18: ...18 Figure 20 Filament Fed Across Hobbed Gear Figure 21 Disengaging the Idler Bar Springs...
Страница 57: ...57 In general you should be able to get within 1 of the correct flow rate with 3 trials...