not to heat too long.
- Pb free solder will tend to splash when heated too high (about
1100°F/ 600°C).
- All products with the printed circuit board with PbF stamp or
printing must be serviced with lead free solder.
When soldering or unsoldering, completely remove all of the
solder from the pins or solder area, and be sure to heat the
soldering points with the lead free solder until it melts sufficiently.
Recommendations
Recommended lead free solder composition is Sn96.5 Ag3.0 Cu0.5.
5. DISASSEMBLY INSTRUCTIONS
5.1. REMOVAL OF MECHANICAL PARTS AND P.C. BOARDS
5.1.1. BACK CABINET (Refer to
Fig. 1-1
)
1. Remove the 4 screws .
2. Remove the screw .
3. Remove the 2 screws .
4. Remove the 2 screws which are used for holding the Back
Cabinet.
5. Remove the AC cord from the AC cord hook .
6. Remove the Back Cabinet in the direction of arrow.
Fig. 1-1
5.1.2. CRT PCB (Refer to
Fig. 1-2
)
CAUTION:
BEFORE REMOVING THE ANODE CAP, DISCHARGE ELECTRICITY
5