MONOTIG 220ip - MONOTIG 220ip AC/DC
EN
www.magmaweld.com
18
USER MANUAL | KULLANIM KILAVUZU
3.1 User Interface
2- TIG Curve
1- Adjustment Button
USAGE INFORMATION
Usage Information
Use the keys to scroll through the parameters in the TTIG curve. The led of the relevant parameter will light up depending on which
parameter is selected.
Initial current
The welding arc will occur at the specified current value. The value is set in terms of %. An initial current occurs below
the specified% value of the main current and allows adjustment from 1% to 99%.
Initial Gas
Darkening - deformation may occur in the welding area, as the shielding gas from the torch reaches the welding area,
which will be more late compared to the arc speed formed. Furthermore, the life of the tungsten tip will be shortened.
Allows adjustment between 0.1-20 sec. By this setting, it is ensured that the gas reaches the welding area before
starting welding.
The adjustment knob allows current setting in all welding methods and parameter changes in all functions.
The setting will be made by turning right and left and the set values will be displayed on the digital display.