7.3 Main unit inspection
GAP INSPECTION
Description
Accept Criteria
1.
Gap between sliding bezel
and housing
GAP
≦
0.9 (mm)
OTHERS
Scratch
Description Accept
Criteria
Class A
Exposure of substrate do not accept
Scratch : L
≦
4mm ,W
≦
0.2mm ,N
≦
2, S
≧
10mm
MI
Class C
Label area don’t care
Exposure of substrate do not accept
Scratch : L
≦
10mm ,W
≦
0.4mm ,N
≦
5, S
≧
5mm
MI
Contamination dot/Granule dot/Cave granule
Description Accept
Criteria
Class A
D
≦
0.5mm ,N
≦
2,S
≧
15 mm (Ignored if D D
≦
0.15mm)
MI
Class C
D<0.9mm ,N
≦
4,S
≧
10 mm
MI
Burr
Description Accept
Criteria
Burr.
Don’t accept hand scrape
MI
Imprint mark
Description Accept
Criteria
Class A
0.25
≦
diameter
≦
0.65mm ,N
≦
3 MI
Bright mark
Description Accept
Criteria
Class A
L
≦
2.5mm,W
≦
0.25mm,N
≦
3 MI
Class C
L
≦
3.0mm,W
≦
0.3mm,N
≦
5 MI
Lint
Description Accept
Criteria
Class A
L
≦
3mm , W
≦
0.2mm ,N
≦
2, S
≧
5 mm
MI
Class C
L
≦
10mm , W
≦
0.3 mm ,N
≦
3 MI