OM-925 Page 38
9-14. Troubleshooting
−
Waviness Of Bead
Waviness Of Bead
−
weld metal that is not parallel and does not cover
joint formed by base metal.
S-0641
Possible Causes
Corrective Actions
Welding wire extends too far out of nozzle.
Be sure welding wire extends not more than 1/2 in (13 mm) beyond nozzle.
Unsteady hand.
Support hand on solid surface or use two hands.
9-15. Troubleshooting
−
Distortion
Distortion
−
contraction of weld metal during welding that forces
base metal to move.
Base metal moves
in the direction of
the weld bead.
S-0642
Possible Causes
Corrective Actions
Excessive heat input.
Use restraint (clamp) to hold base metal in position.
Make tack welds along joint before starting welding operation.
Select lower voltage range and/or reduce wire feed speed.
Increase travel speed.
Weld in small segments and allow cooling between welds.
Summary of Contents for H-10 Gun
Page 24: ...OM 925 Page 20 6 2 Weld Parameter Chart For 115 VAC Model ...
Page 25: ...OM 925 Page 21 217 618 A ...
Page 26: ...OM 925 Page 22 6 3 Weld Parameter Chart For 230 VAC Model ...
Page 27: ...OM 925 Page 23 217 754 B ...
Page 34: ...OM 925 Page 30 217 755 A Figure 8 2 Circuit Diagram For 230 VAC Model ...
Page 45: ...OM 925 Page 41 Notes ...