EasyWeld / HandyWeld 160
STICK (MMAW) Welding 6-12 0-5617
Art # A-05867_AC
Lack of
inter-run fusion
Lack of side fusion,
scale dirt, small electrode,
amperage too low
Lack of root fusion
Lack of fusion caused by dirt,
electrode angle incorrect,
rate of travel too high
Figure 6-30: Example of Lack of Fusion
Description
Possible Cause
Remedy
5 A groove has been formed in the base
metal adjacent to the toe of a weld
and has not been filled by the weld
metal (undercut).
A Welding current is too high.
A Reduce welding current
B Welding arc is too long.
B Reduce the length of the
welding arc
C Angle of the electrode is
incorrect.
C Electrode should not be
inclined less than 45° to the
vertical face
D Joint preparation does not
allow correct electrode angle.
D Allow more room in joint
for manipulation of the
electrode.
E Electrode too large for joint.
E Use smaller gauge
electrode.
F Insufficient deposit time at
edge of weave.
F
Pause for a moment at
edge of weave to allow weld
metal build-up.
Art # A-07714
Figure 6-31: Examples of undercut
Summary of Contents for Cigweld EasyWeld 160
Page 8: ...This Page Intentionally Blank ...
Page 14: ...EasyWeld HandyWeld 160 GENERAL INFORMATION 1 6 0 5617 This Page Intentionally Blank ...
Page 26: ...EasyWeld HandyWeld 160 INSTALLATION 3 4 0 5617 This Page Intentionally Blank ...
Page 32: ...EasyWeld HandyWeld 160 OPERATION 4 6 0 5617 This Page Intentionally Blank ...
Page 56: ...MIG GMAW WELDING 5 24 Manual 0 5617 EasyWeld HandyWeld 160 This Page Intentionally Blank ...
Page 70: ...EasyWeld HandyWeld 160 STICK MMAW Welding 6 14 0 5617 This Page Intentionally Blank ...
Page 78: ...KEY SPARE PARTS 8 4 0 5617 EasyWeld HandyWeld 160 This Page Intentionally Blank ...
Page 80: ...EasyWeld HandyWeld 160 APPENDIX A 2 0 5617 This Page Intentionally Blank ...
Page 83: ...EasyWeld HandyWeld 160 This Page Intentionally Blank ...