Preparation
ElektroPhysik
E-4
5 Preparation before measurement
【
5.1
】
Preparation of the instrument
For the newly purchased instrument, please check the instrument and its
accessory according to the standard delivery table in chapter 9. If you find
it is not the same as the table listed, please contact the manufacture in
time. If the instrument is damaged, please do not use it and contact the
manufacture as soon as possible.
【
5.2
】
Selection of the Probe
Type
Frequency
Measuring range
Temperature
U5.0
5.0MHz
0.8mm
~
300mm
<60
℃
U5HT
5.0MHz
3.0mm
~
100mm
<350
℃
U7.5
7.5MHz
0.65mm
~
50mm
<60
℃
U10.0
10.0MHz
0.65mm
~
20mm
<60
℃
U2.0
2.0MHz
2.0mm
~
500mm
<60
℃
Users can select the suitable probe according to the thickness of the
work-piece to be measured.
U5.0: The probe is used common in many measurements, for example
when the measuring surface is flat or with huge curvature, or the
thickness of the work-piece to be measured is large than 50mm.
U5HT: Mainly used in the thickness measurement when the temperature
is less than 350
℃
U7.5: Mainly used in the measurement of thin wall thickness and
small curvature surface.
U10.0: Mainly used in the measurement of thin wall thickness and
small curvature surface.
U2.0: Mainly used in the measurement of coarse
particles such as cast
iron.