CHAPTER 9
INSTRUCTIONS
Put 5 grams (approx. one teaspoon or half a lid
full) of
ANODIZING POWDER
into the tray.
ATTENTION:
For anodising bigger restorations
(e.g. bars, multi-unit bridges), insert twice the
amount of Anodizing Powder (two teaspoons or a
lid full) into the tray.
Reinsert the tray into the designated fixture in the
Titanium Spectral-Colouring Anodizer.
Place the black cathode at the back, on the inside
of the tray.
Stir the water well a few times until all powder has
dissolved.
Содержание titanium spectral-colouring anodizer
Страница 1: ...titanium spectral colouring anodizer Operator s and maintenance manual...
Страница 3: ...03 03...
Страница 8: ...08 08 KAPITEL...
Страница 15: ...15 15 CHAPTER 2 COMPONENTS COMPONENTS...
Страница 18: ...18 18 KAPITEL 3 TECHNICAL DATA...
Страница 22: ...22 22 KAPITEL 5 OPERATION...
Страница 24: ...24 24 KAPITEL 6 VOLT DIAGRAMS...
Страница 29: ...29 29 CHAPTER 9 INSTRUCTIONS INSTRUCTIONS...
Страница 43: ...43 43 General notes...