55
Cause
Incorrect arc regulation
Solution
Increase the equivalent circuit inductive value setting.
Cause
Insufficient shielding gas.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good conditions.
Cause
Incorrect welding mode.
Solution
Decrease the torch angle.
Insufficient penetration
Cause
Incorrect welding mode.
Solution
Decrease the welding travel speed.
Cause
Incorrect welding parameters.
Solution
Increase the welding current.
Cause Incorrect
electrode.
Solution
Use a smaller diameter electrode.
Cause
Incorrect edge preparation.
Solution
Increase the chamfering.
Cause
Incorrect earth connection.
Solution
Earth the system correctly
Read the paragraph “Installation “.
Cause
Pieces to be welded too big.
Solution
Increase the welding current.
Slag inclusions
Cause Poor
cleanliness.
Solution
Clean the pieces accurately before welding.
Cause
Electrode diameter too big.
Solution
Use a smaller diameter electrode.
Cause
Incorrect edge preparation.
Solution
Increase the chamfering.
Cause
Incorrect welding mode.
Solution
Decrease the distance between the electrode and
the piece.
Move regularly during all the welding operations.
Tungsten inclusions
Cause
Incorrect welding parameters.
Solution
Decrease the welding voltage.
Use a bigger diameter electrode.
Cause Incorrect
electrode.
Solution
Always use quality materials and products.
Sharpen the electrode carefully.
Cause
Incorrect welding mode.
Solution
Avoid contact between the electrode and the weld pool.
Blowholes
Cause
Insufficient shielding gas.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Sticking
Cause
Incorrect arc length.
Solution Increase the distance between the electrode and
the piece.
Increase the welding voltage.
Cause
Incorrect welding parameters.
Solution
Increase the welding current.
Cause
Incorrect welding mode.
Solution
Angle the torch more.
Cause
Pieces to be welded too big.
Solution
Increase the welding current.
Increase the welding voltage.
Cause
Incorrect arc regulation.
Solution
Increase the equivalent circuit inductive value setting.
Undercuts
Cause
Incorrect welding parameters.
Solution
Decrease the welding voltage.
Use a smaller diameter electrode.
Cause
Incorrect arc length.
Solution Increase the distance between the electrode and
the piece.
Increase the welding voltage.
Cause
Incorrect welding mode.
Solution
Decrease the side oscillation speed while filling.
Decrease the travel speed while welding.
Cause
Insufficient shielding gas.
Solution
Use gases suitable for the materials to be welded.
Oxidations
Cause
Insufficient gas protection.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Porosity
Cause
Grease, varnish, rust or dirt on the workpieces to
be welded.
Solution
Clean the workpieces carefully before welding.
Cause
Grease, varnish, rust or dirt on the filler material.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Humidity in the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Incorrect arc length.
Solution
Decrease the distance between the electrode and
the piece.
Decrease the welding voltage.
Cause
Humidity in the welding gas.
Solution
Always use quality materials and products.
Ensure the gas supply system is always in perfect
condition.
Содержание Genesis 4000 MSE
Страница 32: ...32...
Страница 62: ...62...
Страница 212: ...212...
Страница 242: ...242...
Страница 272: ...272...
Страница 302: ...302...
Страница 332: ...332...
Страница 335: ...1 1 1 10 C 40 C 14 F 104 F 25 C 55 C 13 F 131 F 50 40 C 40 00 C 90 20 C 68 F 2000 6500 1 2 10 MIG MAG 335...
Страница 336: ...336 1 3 1 4 11 35 1 5...
Страница 337: ...337 1 6 8 1 7 EN IEC 60974 10 B A A EN60974 10 A pace maker Zmax Ssc Point of Commom Coupling PCC...
Страница 338: ...1 8 IP S IP23S 12 5 mm 60 2 2 1 2 2 10 2 3 400V 230V V 230 400V 338...
Страница 339: ...339 15 15 2 1 5 2 4 MMA 3 4 1 2 WF ARC AIR 5 6 7 ARC AIR 8 9 TIG 10 11 TIG 12 13 14 15...
Страница 341: ...341 8 9 64 3 3 3 4 LCD 1 2 3 1 m min 22 m min Default 1 0 m min 4 5 3 5 MMA TIG DC MIG MAG...
Страница 354: ...5 6 Reset 354...
Страница 355: ...355 encoder...
Страница 356: ...356...
Страница 357: ...357 7 7 1 MMA Hot Start Arc Force antisticking 7 2 TIG TIG Tungsten lnert Gas 3370 C H F lift...
Страница 359: ...359 7 3 MIG MAG MIG SHORT ARC 1a SHORT a SPRAY ARC b SPRAY ARC 1b 2 3 2 3 1a 1b...
Страница 366: ...366 GENESIS 4000 MSE 3x230 400V...
Страница 367: ...367 GENESIS 4000 MSE LCD 3 5 LCD 4 7 3x400V...
Страница 368: ...368 GENESIS 4000 MSE LCD 3 5 LCD 4 7 3x230 400V...
Страница 369: ...369 GENESIS 5000 MSE 3x400V...
Страница 370: ...370 GENESIS 5000 MSE LCD 3 5 LCD 4 7 3x400V...
Страница 372: ...372 GENESIS 4000 MSE LCD 3 5 LCD 4 7 3x400V GENESIS 4000 MSE LCD 3 5 LCD 4 7 3x230 400V...
Страница 373: ...373 GENESIS 5000 MSE 3x400V GENESIS 5000 MSE LCD 3 5 LCD 4 7 3x400V...