TIG DC
- Setting the DOWN SLOPE function
The function is used for the continuous termination of the welding process.
Together with the END CURRENT function, it prevents crater formation at the
end of the weld when properly adjusted. During the set time, the welding
process decreases continuously current to the end current value. Activation is
performed by pressing the control n-encoder one after the other.
TIG HF
N-coder
TIG DC
TIG DC
- Setting the END CURRENT function
The function indicates the current value at which the welding process ends.
Together with the DOWN SLOPE function, it prevents the crater from forming
at the end of the weld when properly adjusted. Activation is performed by
pressing the control n-coder one after the other.
TIG HF
N-coder
TIG DC
TIG DC
- Setting the POST-GAS function
The function ensures protection of the weld after the welding process is com-
pleted and at the same time it cools the tungsten electrode. The low duration
of the function can affect the ignition quality of the arc due to oxidation of the
electrode. Activation is performed by pressing the control n-coder one after
the other.
TIG HF
N-coder
TIG DC
TIG DC
- Setting the 2-STROKE function
The function indicates how the welding process is activated. When using this
mode, it is necessary to press the control button during welding to send a
signal to activate the welding process. Pressing the control button starts the
welding process and activates the sequence of functions. Activation is perfor-
med by pressing the control n-coder one after the other.
TIG HF
N-coder
TIG DC
TIG DC
- Setting the 4-STROKE function
The function indicates how the welding process is activated. In this mode, it
is necessary to press the control button, which sends a signal to activate the
welding process. The PRE-GAS function is then activated, followed by START
CURRENT. When the button is released, the welding process starts by swit-
ching to WELDING CURRENT and activating other active functions gradually.
To complete the welding process, press the control button again to activate
the DOWN SLOPE function and then the END CURRENT function. When the
button is released, the welding process ends and the POST-GAS function is
activated.
TIG HF
N-coder
TIG DC
TIG DC
- Setting the PULSE function
Setting the value determines the lower welding current I
2
of the pulse. Activa-
ting this function reduces the thermal load on the welded material. Activation
is performed by pressing the control n-coder one after the other.
TIG HF
N-coder
TIG DC