19
Problems Causes
Solutions
Internal parts are
damaged during
welding.
The amplitude is too high.
The welding time is too long.
The work-piece absorbs too much
energy. Inappropriate assembly of
the parts; i.e. the distance to the joint
face is too short.
Reduce the amplitude.
Increase the pressure or amplitude to
reduce the welding time.
Adjust the buffer or delay time.
Reduce the amplitude.
Reduce the pressure.
Reduce the welding time.
Use an energy controller.
Make sure the internal parts are
properly assembled.
Isolate the internal parts and housing
Move the internal parts away from
energy area or change the press
position
Design and appliance to offset local
energy.
The area outside the
joint face of the
work-piece is molten
or broken.
The interior angle is too sharp.
The vibration amplitude is too high.
The welding time is too long
Internal stress.
Inappropriate operation conditions.
Blunt the sharp angle.
Reduce vibration amplitude.
Increase vibration amplitude.
Increase the pressure.
Adjust the buffer and delay time.
Review the ejecting conditions.
Review the work-piece conditions.
Check the operation conditions.
Internal parts are
fused.
Internal parts have the same material
as the housing.
Change the material of the internal
parts.
Apply anti-welding agent to the
internal parts.
Содержание KWL3215
Страница 1: ...KWL3215 KWL4215 King Ultrasonic CO LTD Ultrasonic Plastic Welder User s Manual ...
Страница 10: ...9 2 9 2 1 22 23 22 6 Position of Components ...
Страница 11: ...10 組件位置圖 28 29 32 10 30 31 Position of Components ...
Страница 18: ...17 IV Control Wiring Diagram Control System Wiring Diagram ...